③ 晶体生长-液体封装提拉法-LEC

发布时间:2020-06-09

LEC Method   (Liquid Encapsulated Czochralski )


The starting materials (either pre-synthesised polycrystalline chunks or, in the case of semi-insulating GaAs, elemental Ga and As) are placed in the growth crucible along with a pellet of boron trioxide. The crucible is placed inside a high pressure crystal puller and heated up.


At 460°C the boron trioxide melts to form a thick, viscous liquid which coats the entire melt, including the crucible (hence, liquid encapsulated). This layer, in combination with the pressure in the crystal puller, prevents sublimation of the volatile group V element.


The temperature is increased until the compound synthesises (temperatures and pressures are varied depending on which material is being produced). A seed crystal is then dipped, through the boron trioxide layer, into the melt. The seed is rotated and slowly withdrawn and a single crystal propagates from the seed.


Crystal growth is monitored by the use of CCTV cameras and measurements of weights, temperatures and pressures are made at regular intervals.


wps4.jpg


Copyright © 2019 米兰(中国) 版权所有 皖ICP备09007391号-1     皖公网安备 34012302000974号

在线产品展示

设备销售咨询

晶体销售咨询

售后咨询